how to make flux for gold refining
The borax contribution to flux composition can be up to 60% of total flux weight but is typically around 3040% Borates are also used to facilitate the attack of gold ore at a lower temperature and to make the slag more fluid at the furnace operating temperature thus reducing viscosity The benefits of Dehybor in gold refining are numerous